share

Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane CAS NO 110532-34-8


Unit Price:

CAS No.:110532-34-8

Grade:Customizable

Content:Customizable

Brand:Customizable

Packaging:Customizable

Description

Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane (CAS 110532-34-8) is a fatty-acid-modified polyester of the alkyd type, described in the source record as a viscous liquid. It is an amber-colored, high-viscosity organic polymer, consistent with a solvent-free or high-solids alkyd resin body. Its structure combines soybean-oil fatty-acid chains, glycerol and trimethylolpropane polyol segments, and phthalic anhydride-derived aromatic diester units, giving a branched polyester backbone carrying unsaturated fatty-acid side chains. In coating and resin formulation, it serves as a film-forming alkyd binder whose fatty-acid unsaturation supports oxidative curing and whose polyester backbone contributes adhesion, pigment wetting, and film flexibility.

In alkyd resin and coating manufacture, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane serves as a film-forming binder during batch resin let-down and paint milling. The resulting air-drying or stoving coating is used in industrial and architectural surface finishing for protective and decorative film formation.

Application

  • Air-drying protective coatings: In air-drying coating formulation, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane serves as an oxidatively curing alkyd binder, where its soybean-oil fatty-acid unsaturation contributes to crosslinking on exposure to air. The resulting coating is used in industrial and architectural finishing for protective film formation.
  • Industrial paint and primer formulation: In industrial paint and primer formulation, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane serves as a resin binder, where its polyester backbone contributes pigment wetting and film adhesion. The resulting paint is used in metal and general industrial surface protection.
  • Pigment dispersion and mill base preparation: In pigment dispersion and mill base preparation, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane serves as a grinding vehicle, where its viscous polymer body contributes wetting and suspension of pigment particles. The resulting mill base is used in the preparation of pigmented coating systems.
  • Coating film property modification: In coating formulation, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane serves as a modifying alkyd component, where its branched polyester structure and fatty-acid side chains contribute to film flexibility and adhesion balance. The resulting modified coating is used in general protective and decorative finishing.
  • Resin blending and formulation research: In resin blending and formulation research, Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane may be evaluated as an alkyd binder component, where its polyester and fatty-acid segments support studies of cure and film behavior. This is a research evaluation context.

Basic Information

Property Value
Product Name Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane
CAS No. 110532-34-8
Molecular Formula UNKNOWN
Molecular Weight UNKNOWN
Physical Viscous liquid
Color Amber
Chemical Property UNKNOWN
Customization Content/concentration customizable per client specification

Quality Control

The quality of Soybean Oil, Polymer With Glycerol, Phthalic Anhydride And Trimethylolpropane is governed by its branched polyester structure and soybean-oil fatty-acid content, which together determine viscosity, cure behavior, and film properties in coating applications.

Differentiated QC focus Structure, application impact, detection and control
Viscosity and flow behavior The branched polyester backbone and fatty-acid side chains determine the resin's flow characteristics. In coating and paint formulation, viscosity affects pumping, milling, and film leveling; a shifted viscosity can cause uneven film build or poor pigment wetting. Set an agreed viscosity range, qualify incoming resin lots, and trend viscosity against application flow tests. Test by rotational viscometry at a defined temperature.
Acid value Residual carboxylic acid groups from the phthalic anhydride and polyol condensation affect cure and storage stability. In coating formulation, elevated acid value can alter cure rate and reactivity with crosslinkers. Set specification limits on acid value and correlate with cure response. Test by titration with standardized alkali.
Fatty-acid unsaturation and oxidative cure Soybean-oil fatty-acid chains carry unsaturation that drives air-drying crosslinking. In air-drying coatings, low or variable unsaturation can slow dry time and reduce film hardness. Qualify oil-derived raw materials and trend iodine value against drying performance. Test by iodine value titration.
Color and clarity The resin is described as an amber viscous liquid; color development can indicate oxidation or contamination. In clear or light-tinted coatings, excessive color affects appearance. Set agreed color limits and protect from heat and light during storage. Test by visual comparison or colorimetry against a standard.
Volatile matter Residual volatiles can arise from the condensation process or solvent carryover. In coating films, volatiles can cause bubbles, pinholes, or shrinkage during cure. Define devolatilization steps and set limits on volatile content. Test by oven volatilization.
Gel and particulate content Gel particles or foreign matter can arise from polymerization or handling. In thin films and pigmented coatings, particulates cause surface defects. Include filtration and clean packaging, and inspect lots intended for fine film applications. Test by filtration through a defined mesh followed by gravimetric or microscopic examination.

Batch release, COA and traceability. Each batch is released only when it conforms to the agreed specification. The Certificate of Analysis (COA) records the actual analytical methods and results for that released batch. Batch identity and results remain traceable, with lot trending used where it supports consistency review.

Storage

  • Storage conditions: Store in a cool, dry, well-ventilated area. Keep containers tightly closed when not in use.
  • Secure storage: Store in a secure, designated area with access limited to authorized personnel.
  • Incompatible materials: Keep away from strong oxidizers.
  • Handling precautions: Avoid breathing vapors or mist. Use only in a well-ventilated area. Wear protective gloves, protective clothing, eye protection, and face protection. Wash hands thoroughly after handling.
  • Waste disposal: Dispose of contents and container in accordance with local, regional, national, and international regulations.
  • Reference: Refer to the Safety Data Sheet (SDS) for detailed handling and disposal information.

Complete Your RFQ

0/ 2000

why choose us

Trusted Manufacturer

With our own production facilities, we ensure consistent quality, reliable supply, and full traceability.

Rigorous Quality Assurance

Each batch undergoes strict QC, accompanied by COA, MSDS, and full compliance with international standards.

Advanced R&D Expertise

Our in-house lab drives process innovation, new product development, and tailored synthesis solutions.